Hi, Acquired a stainless container, looks like an old keg, it has legs welded on. Inside where the welds show through, its a bit blemished. I would like to convert to a mash tun. If I electric wire brush it to clean up, do you think it will be ok, or is there something I could treat it with that won't leach onto the mash? :)
no palate, no patience.


Drinking - of course

Fil
Telling imaginary friend stories
Posts: 5229
Joined: Sun Oct 16, 2011 1:49 pm
Location: Cowley, Oxford

Re: Stainless

Post by Fil » Tue Oct 21, 2014 6:02 pm

im no expert buit i think using steel wire brushes will premote the stainless steels ability to rust, using a stainless wire brush shouldnt..

if clean and no carbon deposits you may get away with a barkeepers friend poilish, but if crusted up i think its best practice to wear down and re treat with an acid to repacify the stainless.
ist update for months n months..
Fermnting: not a lot..
Conditioning: nowt
Maturing: Challenger smash, and a kit lager
Drinking: dry one minikeg left in the store
Coming Soon Lots planned for the near future nowt for the immediate :(

User avatar
far9410
Even further under the Table
Posts: 2472
Joined: Wed Sep 22, 2010 4:37 pm
Location: Nottingham, usually!

Re: Stainless

Post by far9410 » Tue Oct 21, 2014 6:11 pm

thanks, what acid should i use?
no palate, no patience.


Drinking - of course

Belter

Re: Stainless

Post by Belter » Tue Oct 21, 2014 6:25 pm

pickling paste. Apparently it's hideous stuff and needs to be removed afterwards. I've never used it so no idea if you can just rinse it.

User avatar
far9410
Even further under the Table
Posts: 2472
Joined: Wed Sep 22, 2010 4:37 pm
Location: Nottingham, usually!

Re: Stainless

Post by far9410 » Tue Oct 21, 2014 9:22 pm

Bloody hell!, I thought it might be easy, just looking at pickling paste cosh sheets!
no palate, no patience.


Drinking - of course

User avatar
barneey
Telling imaginary friend stories
Posts: 5423
Joined: Mon Jul 25, 2011 10:42 pm
Location: East Kent

Re: Stainless

Post by barneey » Tue Oct 21, 2014 11:49 pm

Pickling paste, is straight forward to use, paint it on,,,,,, wait,,,,,, & wash off.

Don't paint yourself (skin will go yellow), don't breath in the fumes, just read the instructions / sheets for it.
Hair of the dog, bacon, butty.
Hops, cider pips & hello.

Name the Movie + song :)

User avatar
far9410
Even further under the Table
Posts: 2472
Joined: Wed Sep 22, 2010 4:37 pm
Location: Nottingham, usually!

Re: Stainless

Post by far9410 » Wed Oct 22, 2014 4:38 am

Ok thanks, I'll have a go :?
no palate, no patience.


Drinking - of course

Fil
Telling imaginary friend stories
Posts: 5229
Joined: Sun Oct 16, 2011 1:49 pm
Location: Cowley, Oxford

Re: Stainless

Post by Fil » Wed Oct 22, 2014 4:24 pm

if you can find it in anything other than industrial volumes..
i had to revert to an acid based automotive ruste removal gel, (fingers crossed so far so good..)
ist update for months n months..
Fermnting: not a lot..
Conditioning: nowt
Maturing: Challenger smash, and a kit lager
Drinking: dry one minikeg left in the store
Coming Soon Lots planned for the near future nowt for the immediate :(

User avatar
Buckie Brewer
Piss Artist
Posts: 131
Joined: Wed Jan 11, 2012 8:06 pm

Re: Stainless

Post by Buckie Brewer » Thu Oct 23, 2014 7:03 pm

If the blemish you are describing is like this

Image

then you can clean it up with these and a bit of elbow grease.

http://www.amazon.co.uk/gp/product/B00G ... 0Z3DFP2PC5

User avatar
far9410
Even further under the Table
Posts: 2472
Joined: Wed Sep 22, 2010 4:37 pm
Location: Nottingham, usually!

Re: Stainless

Post by far9410 » Mon Oct 27, 2014 9:10 pm

Hi Thanks, I will give that a try first
no palate, no patience.


Drinking - of course

User avatar
scotia
Hollow Legs
Posts: 442
Joined: Wed Aug 14, 2013 6:42 pm
Location: Scottish borders
Contact:

Re: Stainless

Post by scotia » Tue Oct 28, 2014 8:20 am

I find that the black scotchbrite pad is better for stainless the green and marone are better for alloy, there is also an abrasive block manufactured by Garrison which can be sanded to a sharp point if needed to get into tight corners. the Blue one is a good all rounder.
http://www.amazon.co.uk/Garryson-Garryf ... B0001P08UQ

I had a rep in showing a new product last week which was a strip you placed onto the weld left for 15 mins then wiped off with a neutraliser at £40 for a 25mtr roll and £20 for the neutraliser he was soon on his way. I also have what they call tigbrush which uses an electrolyte and ac/dc current depending on application but ye canny beat pickling paste for ease and result,